Application:
Alumina silicon carbide brick can be used as the supporting material for the lining of wire quenching heating furnace and the corundum silicon carbide side rail brick for steel rolling heating furnace. It can also be used as kiln furniture for ceramic firing.

High Working Temperature

Good Thermal Shock Resistance

Great Wear Resistance

High Temperature Compressive Strength
Technical Data:
| Item | Gm1650 | Gm1600 | Gm1550 | |
|---|---|---|---|---|
| Al₂O₃, % | ≥ | 65 | 63 | 60 |
| Bulk Density, g/cm³ | ≥ | 2.65 | 2.60 | 2.55 |
| Apparent Porosity, % | ≤ | 17 | 17 | 19 |
| Cold Crushing Strength, MPa | ≥ | 85 | 90 | 90 |
| 0.2MPa Refractoriness Under Load, °C | ≥ | 1650 | 1600 | 1550 |
| Thermal Shock Resistances (1100°C, Water Cooling), Cycle | ≥ | 10 | 10 | 12 |
| Resistance to Abrasion at Ambient Temperature, cm³ | ≤ | 5 | 5 | 5 |